HARDENING THE ALLOY STEEL BY CYANIDING AND WATER QUENCHING

  • О. А. Касилов Kherson State Maritime Academy
  • Б. В. Малыгин Kherson State Maritime Academy
Keywords: alloy steel, cyaniding, hardening, surface hardness, wear resistance

Abstract

Hardening of 20 grades of structural and instrumental steels by liquid cyaniding in isothermal conditions at 800°С and by stepped oil quenching at 820-870 °С in salt bath have been compared with standard quenching of optimum temperatures. Hardening effect has been obtained for all steel grades. Slow releasing to reduce internal hardening stress softens the steel by 2-4 units HRCЭ.

References

Конторович И. Е. Термическая обработка стали и чугуна / И. Е. Конторович. – М. : Металлургиздат, 1950. – С. 291-301.

Вязников Н.Ф. Термическая обработка стали / Н. Ф. Вязников. – М. : Металлургиздат, 1961. – С. 216-220.

Металловедение и термическая обработка стали : справочник. – Том 2. – М. : Металлургиздат, 1962. – С. 1016-1024.

Самохоцкий А. И. Технология термической обработки металлов / А. И. Самохоцкий. – М. : Машгиз, 1962. – С. 172-185.

Гуляев А. П. Металловедение / А. П. Гуляев. – М. : Металлургия, 1977. – С. 336-338.

Лахтин Ю. М. Химико-термическая обработка металлов / Ю. М. Лахтин, Б. Н. Арзамасов. – М. : Металлургия, 1985. – С. 138-141.